无溶剂液体环氧涂料在天然气管道热煨弯管外防腐层修复中的应用
The Application of Solvent-Free Liquid Epoxy in External Anti-Corrosive Coating Overhaul of Hot Induction Bends in Gas Pipelines
摘要: 长输管道广泛采用双层熔结环氧粉末涂层作为热煨弯管的外防腐层,在长期阴极剥离及地下水浸泡下,双层熔结环氧粉末涂层与热煨弯管钢管表面易出现粘结力不足现象,造成阴极保护电流损失,需要进行热煨弯管外防腐层修复。通过对比修复材料优缺点和在役天然气管道现场实际,推荐选取无溶剂液体环氧涂料进行修复;为增强机械强度和密封性能,采用聚丙烯胶粘带作为外防护带。介绍了修复材料技术要求,简述了施工流程和施工方案,阐述了质量控制方法。通过实际应用取得了良好的修复效果,保障了管道的安全运行。
Abstract: Double-layer fusion bonded epoxy is widely used as external anti-corrosive coating for hot induction bends in long-distance pipelines. When it is used under the condition of cathodic delamination and groundwater immersion, the adhesive strength between double-layer fusion bonded epoxy and the surface of hot induction bend will become insufficient, which leads to the damage of current cathodic protection; therefore, it is imperative to repair the external anti-corrosive coating. By comparing advantages and disadvantages of the repairing materials and practical condition of gas pipeline in service, it is advisable to choose solvent-free liquid epoxy as the repairing material. In order to enhance the mechanical strength and sealing performance, polypropylene adhesive is used as the outer protective belt. This thesis introduces technical indicator of repairing material, expounds construction procedure and construction scheme, and elaborates quality inspection method. This repairing technology has achieved ideal result in practical application and ensured the safe operation of gas pipelines.
文章引用:李世龙. 无溶剂液体环氧涂料在天然气管道热煨弯管外防腐层修复中的应用[J]. 石油天然气学报, 2021, 43(2): 112-119. https://doi.org/10.12677/JOGT.2021.432020

参考文献

[1] 张玉志, 邵建, 陈洪源, 等. 国内外管道外防腐层应用现状与发展趋势[J]. 油气储运, 2011, 30(11): 845-847.
[2] 孙丽华, 田艳玲, 邢战刚, 等. 钢质热煨弯头双层环氧粉末涂层[J]. 油气储运, 2005, 24(11): 50-52.
[3] 窦宏强, 詹胜文, 刘佳, 等. 油气长输管道热煨弯管防腐层现状及展望[J]. 石油与天然气化工, 2020, 9(1): 77-81.
[4] 牟华, 杨浩, 周德志. 钢制管道热煨弯管外防腐的现状与展望[J]. 天然气与石油, 2006, 24(2): 27-29.
[5] 彭真, 蒋宏业, 敬玉娟. 热煨弯管单层FBE外缠聚乙烯复合带防腐技术[J]. 天然气工业, 2016, 36(2): 98-101.
[6] 刘小利, 张晓东, 邓震, 等. 钢质热煨弯管的环氧粉末+聚丙烯胶带涂层防腐结构施工技术[J]. 石油工程建设, 2011, 37(1): 61-63.
[7] 刘玲莉, 张永盛, 王富才, 等. 管道防腐层大修案例分析及大修选段原则[J]. 油气储运, 2007, 26(3): 23-25.
[8] 油气储运专业标准化技术委员会. SY/T 5918-2017埋地钢质管道外防腐层保温层修复技术规范[S]. 北京: 石油工业出版社, 2017.
[9] 姜有文, 黄光前, 李菲菲, 等. 埋地保温管道防腐蚀保温层修复技术[J]. 腐蚀与防护, 2018, 39(12): 957-961.
[10] 杨雪梅, 刘玲莉, 刘志刚, 等. 我国油气管道防腐层大修技术现状[J]. 油气储运, 2002, 21(10): 7-12.
[11] 陈洪源, 张国权, 刘玲莉, 等. 冷缠胶带在管道防腐层大修中的适用性[J]. 油气储运, 2007, 26(6): 52-53.
[12] 张秀云, 韩建波, 张羽, 等. 液体环氧补口技术在长输管道中的质量控制[J]. 天然气与石油, 2018, 36(2): 89-95.
[13] 许传新, 程书旗, 丁春霖, 等. 在役埋地管线防腐层大修技术[J]. 腐蚀与防护, 2006, 27(12): 645-647.