Sr对Mg-6Zn-2Al-2Ca合金显微组织的影响
The Effect of Sr Addition on the Microstructure of Mg-6Zn-2Al-2Ca Magnesium Alloy
摘要: 采用扫描电镜、X射线衍射仪和光学显微镜研究了Mg-6Zn-2Al-2Ca-xSr (x = 0, 0.5, 1, 2, 3)合金随Sr的含量变化组织形貌的演化规律。实验结果表明:0.5%Sr可以抑制β-Mg17Al12相的形成;Sr的加入,具有增加Mg-6Zn-2Al-2Ca液态金属成分过冷的能力,使胞状组织向树枝状组织发展,枝晶组织随Sr含量的增加而得到细化。当Sr含量达到3%时,形成非枝晶状组织。当Sr含量超过2%时,组织中板块状Mg17Sr2相尺寸明显增大,对组织的演化规律进行了讨论。
Abstract: The effect of Sr addition on microstructure evolution of Mg-6Zn-2Al-2Ca-xSr (x = 0.5, 1, 2, 3) alloys was investigated by using scanning electron microscope (SEM), X-ray diffraction (XRD) and optical microscope. The results show that the 0.5% Sr addition can restrain the formation of β-Mg17Al12 phase. The constitutional undercooling increases with Sr addition, which changes the structure from cellular to dendritic. The dendritic structure becomes more refinement with Sr addition. Furthermore non-dendritic structure is formed when Sr content is 3%. However, a paddle Mg17Sr2 structure was observed when Sr content is 2% and its size increases with Sr. The structure evolution of Mg-6Zn-2Al-2Ca alloy with Sr addition was discussed.
文章引用:邱克强, 张伟刚, 任英磊, 尤俊华. Sr对Mg-6Zn-2Al-2Ca合金显微组织的影响[J]. 材料科学, 2012, 2(1): 47-51. http://dx.doi.org/10.12677/ms.2012.21008

参考文献

[1] O. Mihriban, Pekguleryuz, M. Dierks, et al. Creep resistant magnesium alloys for power-train applications. Proceedings of Annual World MA 2001 Magnesium Conference, 2001, 32(1): 37-45.
[2] A. Z. Munit, C. Cotler, A. Stem, et al. Mechanical properties and microstructure of gas tungsten are welded magnesium AZ91D plates. Materials Science and Engineering, 2001, 302(1): 68-73.
[3] 郭旭涛, 李培杰, 曾大本等. 稀土在耐热镁合金中的应用[J]. 中国稀土学报, 2002, 2: 63-67.
[4] 周涛, 陈振华, 夏华等. Ca及其含量对快速凝固Mg-Zn合金组织和性能的影响[J]. 材料热处理学报, 2011, 32(8): 60-67.
[5] 李长春, 李全安, 张兴渊等. Ca在耐热镁合金中的应用[J]. 热加工工艺, 2010, 39(16): 34-36.
[6] 薛山, 孙扬善, 丁绍松等. Ca和Sr对AE42合金蠕变性能的影响[J]. 东南大学学报(自然科学版), 2005, 35(2): 261-265.
[7] L. Y. Wei. The intergranular microstructure of cast Mg-Zn and Mg-Zn-RE alloy. Materials Transactions A, 1995, 26(8): 1947- 1953.
[8] 李淑琼, 严红革, 陈吉华等. Sn和Ca对ZA62合金组织稳定性的影响[J]. 材料热处理工艺, 2008, 37(4): 5-9.
[9] X. G. Liu, X. D. Peng, W. D. Xie, et al. Preparation technologies and applications of strontium-magnesium master alloys. Mater Science Forum, 2005, 31: 488-499.
[10] J. Bai, Y. S. Sun and S. Xun. Microstructure and tensile behavior of Mg-4Al based magnesium alloys with Alkaline-earth elements Sr and Ca additions. Materials Science and Engineering A, 2006, 419: 181.
[11] 周晓莉. 无机化学[M]. 北京: 化学工业出版社, 2009.
[12] 白星, 胡文俊, 张立强等. Sr对AZ91镁合金组织及力学性能的影响[J]. 中国有色金属学报, 2008, 18(9): 1596-1601.
[13] X. Q. Zeng, Y. X. Wang, W. J. Ding, et al. Effect of strontium on the microstructure, mechanical properties and fracture behavior of AZ31 magnesium alloys. Metallurgical and Materials Transactions A, 2006, 37(4): 1333-1341.
[14] Y. C. Lee, A. K. Dahle and D. H. Stjohn. The role of solute in grain refinement of magnesium. Metallurgical and Materials Tran- sactions A, 2000, 31(11): 2895-2906.
[15] 冒国兵, 刘琪. Sr对AZ91镁合金铸态组织和力学性能的影响[J]. 铸造, 2010, 59(6): 614-617.
[16] M. Aljarrah, U. Aghaulor, M. Medraj, et al. Thermodynamic assessment of the Mg-Zn-Sr system. ScienceDirect on Site, 2007, 15(1): 93-97.