环境温湿度变化对PA6-GF15韧性影响
Investigation on Environmental Change to PA6-GF15 Toughness Property
摘要: 汽车座椅及内饰产品中一些零件常用到PA复合材料,其干态与湿态条件下的韧性差异很大。本文研究了PA6-GF15样条的含水率受环境温湿度的变化规律及对缺口冲击强度的影响,结果表明随时间的变化,在干燥的环境中含水率逐渐降低,在湿润的环境中含水率会缓慢上升;样条含水率发生变化后,低温缺口冲击强度变化不大,室温下的缺口冲击强度会随含水率的变化而发生显著变化。
Abstract: PA composite always used by seats and interior parts, in which toughness property is a significant difference between the condition of dry and humid. In this paper, we studied the environmental temperature and humidity changes effect to PA6-GF15 samples performance such as water absorption and notched impact. The results show that water content of PA6-GF15 samples gradually reduced in the dry environment and increased in humid environment; at low temperature, notch impact strength was not obviously affected by water absorption but obviously at room temperature.
文章引用:李淑莹, 丁慧敏, 国鸽, 高华春, 张丽丽. 环境温湿度变化对PA6-GF15韧性影响[J]. 应用物理, 2020, 10(4): 257-261. https://doi.org/10.12677/APP.2020.104032

参考文献

[1] 吕桂英, 朱华, 林安, 等. 现代测试技术在尼龙6老化研究中的应用[J]. 工程塑料应用, 2006, 34(2): 64-66.
[2] 谭寿再, 杨崇岭, 李建刚. 纳米碳酸钙对PA6/PP共混合金的性能影响[J]. 工程塑料应用, 2011, 39(12): 31-34.
[3] 黄虹文, 刘长维, 韦加崇. 原位聚合La2O3/MC尼龙复合材料的制备与性能[J]. 塑料, 2008, 37(3): 69-71.
[4] 杨明山. 尼龙6与改性PP的共混研究[J]. 高分子材料科学与工程, 1996, 12(3): 85-89.
[5] 宁冲冲, 崔益华, 吴银财, 徐娟, 等. 降低尼龙制品吸水率的研究进展[J]. 塑料科技, 2013, 41(1): 105-108.